morphogen.coupling.ageing

Properties that evolve with chemical ageing, and their maps in microstructures.

An ageing tracer (the amide concentration of oxidized epoxies, Ernault et al. 2019; the degree of polymerization of cellulose in paper, Vibert et al. 2024; an absorbed amount of oxygen or water) sets the local parameters through measured laws (PropertyLaw: piecewise linear tables, constant beyond them). A field of the tracer in a microstructure (an oxidation or diffusion profile) is binned into graded phases (graded_materials()) that the homogenization solvers and the exports take like any other phases; a chemical shrinkage or a swelling becomes the expansion of the graded phases under a unit change of temperature (Loading(..., temperature=1)).

class morphogen.coupling.ageing.PropertyLaw(tracer: tuple, values: dict = <factory>)[source]

Bases: object

Material parameters (young, poisson, conductivity, expansion…) as piecewise linear functions of a tracer: values[name][i] at tracer[i] (increasing), constant beyond the table.

material(x: float, **fixed) → Material[source]

The material at the tracer value x (fixed: the other parameters).

morphogen.coupling.ageing.graded_materials(phases, tracer, laws: dict[int, PropertyLaw], materials: dict[int, Material] | None = None, *, levels: int = 16, first_label: int | None = None, **fixed) → tuple[VoxelImage, dict[int, Material]][source]

Graded phases of an ageing microstructure: the voxels of each phase with a law in laws are binned by their tracer value into levels classes of equal width, each a new phase whose material is the law at the middle of its class (fixed: parameters common to all, e.g. poisson=0.37); the other phases keep their labels and materials. Returns the label image and the materials of all its labels.

class morphogen.coupling.ageing.Hydrolysis(dp0: float = 1500.0, rate: float = 1e-10, temperature: float = 353.15, activation_energy: float = 110000.0, critical_dp: float = 750.0)[source]

Bases: object

Chain scissions of cellulose by acid hydrolysis, Ekenstam’s law: 1/DP(t) - 1/DP(0) = k t (k in 1/s at temperature, Arrhenius with activation_energy J/mol). Vibert et al. (2024) found that the mechanical properties of aged papers fall faster below a critical degree of polymerization critical_dp (about 750), whatever the ageing (hydrolysis or oxidation): the fibres embrittle, more than their bonds.

rate_at(temperature: float | None = None) → float[source]
dp(t, temperature: float | None = None) → ndarray[source]

Degree of polymerization after the time t (s).

scissions(t, temperature: float | None = None) → ndarray[source]

Scissions per initial chain, DP(0)/DP(t) - 1.

time_to(dp: float | None = None, temperature: float | None = None) → float[source]

Time to reach the degree of polymerization dp (default: the critical one).